StuckExperimental or Measurement ProblemNov 20Delamination after thermal cyclingOur printed Ti-6Al-4V lattices delaminate from the build plate coating after 200 thermal cycles (−40 to 150 °C). Tried a bond coat; no change. Has anyone solved this?
StuckData Analysis & InterpretationOct 23Porosity measurements disagree between CT and ArchimedesMicro-CT gives 0.4% porosity on our printed Ti-6Al-4V; Archimedes gives 1.1%. Which should we trust for fatigue modeling?